Wenzhou Kaixin Metal Co., Ltd.

 

TP317LN Stainless steel 1.4434 (UNS 31753) Manufacture in china

Roostevabast terasest klass

TP317LN Roostevaba teras 1.4434 (UNS 31753)

Mis on roostevaba teras 317LN?

Stainless steel 317LN is a nitrogen alloyed austenitic stainless steel having high nitrogen content than other austenitic stainless steels. It has higher yield and tensile strength than 317L. This low carbon grade steel provides resistance to sensitization during welding and thermal processes. Low carbon content in its composition makes the alloy resistant to inter granular corrosion. It also offers excellent corrosion resistance to organic, sulfuric and phosphoric acids.

317LN roostevaba teras 1.4434 Valmis toodete vorm

  • Spiraal - ribad
  • Foolium: Ulbrichi roostevabast terasest traat - Profiil
  • Ümmargune
  • Tasane
  • Ruut

Taotlused 317LN roostevaba teras

  • Chemical processing equipment
  • Toiduainete töötlemise seadmed
  • Pharmaceutical manufacturing equipment
  • Marine engines and exhaust systems
  • Offshore drilling platforms
  • Aerospace components
  • Power generation equipment
  • Soojusvahetid
  • Boilers
  • Turbines
  • Piping systems
  • Reactors
  • Tanks
  • Klapid
  • Vedrud

Equivalents of grade 317LN

JIS G4304ASTMUNSKSISO DesignationAISI
SUS317LN317LNS31753STS317LNX2CrNiMoN18-12-4317LN

Keemiline koostis

ElementsFeCrNiMoMnSiNPCS
Min (%)57.918113.0--0.1---
Max (%)67.920154.02.00.750.220.0450.0300.030

Mehaanilised omadused 

OmadusedMetrilineImperial
Tensile strength≥590 MPa≥85600 psi
Yield strength≥285 MPa≥41300 ksi
Modulus of elasticity200 GPa29000 ksi
Shear modulus77 GPa11200 ksi
Poissons ratio0.2990.299
Elongation at break≥40%≥40%

Füüsikalised omadused

TP317LN Stainless steel 1.4434 (UNS 31753) Physical Properties
TP317LN Stainless steel 1.4434 (UNS 31753) Physical Properties

Manufacturing process

The properties of 317LN is similar to other conventional austenitic stainless steels, and can therefore, be fabricated in a manner similar to alloys 316L and 317L. Heat treatment of 317LN can be carried out at temperatures ranging from 1080 to1175°C (1975 to 2150°F) followed by rapid water quenching. This grade is not hardenable.